title: "Ambrell Video | Hardening with Induction"
description: "Induction heating is used to harden a a metal cross member. It is heated to 1600 deg. F in only 5 seconds!"
type: article
version: 2
version_id: "e55be318-5a8d-4d33-bc33-aaabade68b68"
generated_at: "2026-04-29T12:16:38.811Z"
date_modified: "2026-01-27T15:50:56.130Z"
language: en-us
reading_time: "1 min"
word_count: 48
keywords: ["Ambrell Video", "Hardening with Induction"]
url: "https://www.ambrell.com/induction-heating-videos/hardening-with-induction"
---

# Ambrell Video | Hardening with Induction

> Induction heating is used to harden a a metal cross member. It is heated to 1600 deg. F in only 5 seconds!

## Key Takeaways

- Induction heating is used to harden a a metal cross member
- Induction heating is used to harden a a metal cross member
- Induction heating is used to harden a a metal cross member

# Hardening with Induction

Induction heating is used to harden a a metal cross member. It is heated to 1600 °F in only 5 seconds!

---